Carlie Posted June 6, 2019 Report Share Posted June 6, 2019 I have 3 cups that I over-glazed and almost got stuck to the kiln . I was wondering if there was any way I could get it off some of the excess post-firing. Can I rub some of it off with sandpaper? Any suggestions? Link to comment Share on other sites More sharing options...
liambesaw Posted June 6, 2019 Report Share Posted June 6, 2019 I use a diamond disc on my wheel, works good but takes time, I have 280 grit for grinding my bottoms, 600 for a polished surface after Link to comment Share on other sites More sharing options...
neilestrick Posted June 7, 2019 Report Share Posted June 7, 2019 The grey-green Dremel grinding stones work well, if you have a Dremel tool Link to comment Share on other sites More sharing options...