Momo Posted April 12, 2019 Report Share Posted April 12, 2019 Hi all, I'm just wondering what the lowest acceptable bisque firing temperature would be - and why? I usually single-fire my pottery but occasionally I like to brush on and sponge off a watered down underglaze (so it clings to the texture) before glaze firing. So...could I technically bisque fire at a much lower temperature because all I need is a porous surface? Thank you in advance. Link to comment Share on other sites More sharing options...
Min Posted April 12, 2019 Report Share Posted April 12, 2019 There might not be a one size fits all answer to your question. You could fire to ^022 (approx 1090F) but the bisque might be too porous or fragile for your techniques. Link to comment Share on other sites More sharing options...
Momo Posted April 13, 2019 Author Report Share Posted April 13, 2019 I fired to 700 celsius and it turned out fine - so that's good to know. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.