Jill1989 Posted January 6, 2019 Report Share Posted January 6, 2019 I work w/ C6 clay and found a C5 glaze that I love. If I glaze fire to C5 will there be any complications? Link to comment Share on other sites More sharing options...
neilestrick Posted January 6, 2019 Report Share Posted January 6, 2019 Shouldn't be a problem, but it wouldn't hurt to do an absorption test to be sure. Link to comment Share on other sites More sharing options...
Min Posted January 6, 2019 Report Share Posted January 6, 2019 Or try at test with your ^5 glaze fired to ^6, might be okay too. Welcome to the forum Link to comment Share on other sites More sharing options...
Chilly Posted January 7, 2019 Report Share Posted January 7, 2019 Test, test, test. Only way you'll really know. Try testing both ways, higher and lower. Try testing with horizontal and vertical tests. Use wasters under all tests. I sometimes enjoy the testing process as much as the final results. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.