erauschceramics Posted September 20, 2018 Report Share Posted September 20, 2018 I am interested in finding a cone 5/6 clear glaze that will mimic the 'orange peel' texture that happens during a cone 10 Salt firing. Does that magically exist already? Link to comment Share on other sites More sharing options...
Babs Posted September 20, 2018 Report Share Posted September 20, 2018 I've succeeded with some stuffed up glaze applications....... Link to comment Share on other sites More sharing options...
liambesaw Posted September 20, 2018 Report Share Posted September 20, 2018 I've had a recipe I added too much zircopax to go orange peel, but that's just unhealed bubbles that popped Link to comment Share on other sites More sharing options...