I hope you can reassure me I am ok. My old kiln quit after 6 hours at 1353 degrees for bisque set for 10 hr firing. It’s a speckled brown stoneware clay. It’s now very pink. It does appear to be ceramic and some of the pieces ring when tapped.
Should I refire and do I do a complete 10 hr firing or can I do like. Quick 4 or 7 hour. I have an old Gare kiln using. Ramp master 2 controller. It failed at the breaker which we think was old
thanks for your help