Help! I'm trying to make a large circular slab piece ( on request) which is around 35cm across. I have attempted this 3 times and am now able to successfully bisque fire it, but during glaze firing ( to 1250) it has split, every time. Any suggestions that I might be able to implement, given I am a hobby potter using an electric kiln with preset firing programmes..?
-
Hi Catherine, not quite sure how you ended up posting to my profile but you should start a new thread in Studio Operations and Making Work - https://community.ceramicartsdaily.org/forum/22-studio-operations-and-making-work/ should be an orangeish button saying "start new topic"
-
Managed to double post somehow...
-
Thanks- not used to using this . I appreciate you getting back to me.
-