  1. Good day, I am new at pottery and have a huge problem finding suitable transparent/clear glaze and underglaze for my body of clay. I use 254 and 240 from georg & schneider. I always get crazing and pottery keeps on cracking for days. Any suggestins what should I use in terms of glaze and underglaze?
×
×