I'm not a patient human, I'm just going to let people know that they are hand made and therefore people seem to like them more. Crappy imperfections on the pot/mug seem to make people like them more. However I have to make the glaze spot on.
I'm using terracotta or earthenware. The things that I make are mugs and bowls about 6 inches across. I would send pictures but what I want is generally low quality
Hi I'm a newbie and have set up in the garage. My question is what's a good set up to dry my work? It's takes about 3 days to become leather hard. It's taking soooo long