  1. So I saw a lot of ceramics like this in Instagram and Pinterest , I tried to contact they didn't answer me , I like to know how can I use glaze like that , If Im right I figure out she use slip , and it's a matte glaze but how can I make that rough surface ? Or some places gets brownish color , there is no order in white colored but in the videos she posted , she put used slip or glaze with same amount everywhere , so anybody can help me ? Her Instagram is : Eleaceramics
  2. Thanks everybody I find kind of solution that works for me , 50% clay dust and 50% titanium or 50% clay dust and 50% opak ( it's a white glaze we called it opak ) I'm gonna try other ways you recommend if I can get my hand to materials , we have some powder called talc , we prevent clay from sticking to other things , if it's a right talc you guys taking about
  3. The traditional Clay is brownish and should be cock on 900 to 1000 , beside that there is something supplier calls Ceramic clay , Ceramic clays can be find in white and black color but after cocking both turn white , ceramic clays cocking temperature is 1000 to 1150 or something like that , I can not find any stoneware clay at least with a definition that I read in english , but this is a products I get access to . So I like to use engobe technic for decoration on our traditional clay , but problem is I cannot find white clay with same temperature.
  4. I have a problem, I work with a red clay that has a cooking temperature of 950 to 1000, now how do I make a slip for it? I do not find any clay that is this degree of baking and is white
×
×