Everything posted by Min
-
My dad uses the expression "money for old rope" a fair bit. My QOTW would be do you make anything that is easy and quick to make but looks like it's more work than it is? If you sell your work this would include being able to charge about the same for a pot as what a more labour intensive pot would fetch. Money for old rope pots.
-
When looking for answers it’s very helpful for all of those who try and help or contribute to a post to have a rough idea of the original poster's experience or knowledge base in regards to their question. If a member has been posting here for a while we can get an idea of their experience and try and tailor our replies to reflect what we surmise to be their knowledge / experience level. This is really hard to do with new members or those who post infrequently! We all try to be as helpful as possible but the answers can, at times, be more confusing than the questions. Mentioning your experience should get you more relevant answers than us overloading information but we can’t do this without an idea of knowledge / experience. Including as many details as possible, photos if relevant, and knowledge / experience relevant to the question being asked will hopefully aid everyone is both giving and receiving their questions and comments. Thank you
-
Haha, I wish! Most of the stuff I order in is duty free already, it's the surcharge the private companies charge that is the killer. I had some stuff shipped from Bailey's, most of it came to the drop shipment place I use in Lynden WA except once they had to ship a splashpan separately and they shipped it to my home. The surcharge was more than the splashpan (around $40). Shipments under 20- CA have no duty or taxes added.
-
@Callie Beller Diesel, do you have Chit Chats in Calgary? I've got a family member who used them to ship books from Vancouver to places in the US. He would drop off the boxes in Burnaby (Vancouver suburb) then Chit Chats took them down across the line and shipped them via USPS. It cost him around $2- per box plus whatever the US shipping was. I don't know if they are still in business or not, this was going back a few months. From their website: @liambesaw, we do have UPS but it's silly expensive, as is Purolator or Fed Ex and Canada Post. The cross border fees that UPS, Purolator or Fed Ex charge are crazy, they bill whatever the duty is then tack on a huge surcharge. If there isn't any duty they still add a ridiculous surcharge. I NEVER get anything shipped from the US to here in Canada unless its via USPS.
-
Thanks for sharing this Karen! I was thinking that it would be easy to adapt syringes to make other sizes too.
-
Looks like cobalt will be mined in northern Ontario again. If our suppliers will have access to it that would be a positive. https://www.northernontariobusiness.com/industry-news/mining/engineers-go-to-work-on-cobalt-refinery-restart-1673295 I never heard back from the stain manufactures I contacted regarding Cd inclusion stains. I spent a fair bit of time trying to track down information to counter what Tony Hansen writes as to the processing practices of it but came up empty. I think this comes down to where you draw the line in the sand as to what we are okay with using. Cd inclusion stains are made for the ceramics industry; they are not made for a larger industry and ceramics gets a tiny portion of it like most of the minerals we use. I've made the decision to stop buying the underglazes that I was using that include them.
-
For holding flower stems? edit: another guess, something for running yarn through for weaving or looming?
-
@Hulk, don't know if this is something you might be interested in but there is a mentorship program available for free if you are current member of ICAN. Listing of current mentors. Mentors and mentees can get in touch via email, phone, skype or in person. I know of one lovely man who is a member of this forum who mentored a woman from my area. I know it meant the world to her before she passed away to have this connection.
-
Thank you Liam and Hulk! Ouch on the hornet sting Liam. There have been a couple Giant Asian Hornets found here recently, really nasty things with a wingspan of about 3". Those shelves are just odd boards and strips of ply with leftover laminate flooring on top of them so I can wipe them down without the sponge getting caught up on the rough boards. Batts are homemade plaster ones, no pins, stick to a Xiam Batemate.
-
-
Frank Gaydos was generous enough to allow us to post his Frit Substitution Chart here on the forum. It contains a chart of some common frits with substitutions plus a lengthy list of frits with their composition. Included are Ferro, Hommel, Pemco, PotClays and PotteryCrafts. I've added a link to the DigitalFire reference list of frits to include Fusion and other frits not included in the Frank Gaydos pdf. (direct permission from the author, Frank Gaydos, obtained prior to posting here) Frank Gaydos Frit Substitution Chart Frits.pdf edit: posting pdf's is new here, it looks like you need to be signed in to open the pdf link
-
I have contacted both Mason and Ferro (includes Cerdac, Degussa and Drakenfeld stains) requesting info on their stewardship practices in regards to cadmium inclusion stain manufacturing. If I hear back from them I'll post their replies here. Does anybody have any literature on the processing practices of cadmium inclusion stains? From this link at Digitalfire: "... stain is further rendered safer-to-use by washing with water or weak acid to remove any soluble uncombined compounds (e.g. cadmium or soluble impurities). This washing process does produce toxic byproducts that can only be tolerated in certain countries (e.g. India, China)." Considering the toxicity of Cd this is an ethical issue for me, if Mason or Ferro do corroborate what Tony Hansen is saying on Digitalfire then I will no longer be buying underglazes that use Cd stains. I do hope you are correct Pres in that the mining practices will be changing and child labour will no longer be part of the equation. I will gladly pay more for it if I know it's ethically sourced. BTW @liambesaw, even at $50 lb that's still about 1/2 of what it costs if I buy it from my local ceramic supply place (which I don't). From my local place's catalogue "Cobalt Carbonate .................. 500 grams 92.10 Cobalt Oxide ...............500 grams 102.00 "
-
I've got a girlfriend who has signed up for a Dawn Candy workshop, on the materials list she said she uses Amaco Velvets but can use other brands. Sean O'Connel's website has the glaze recipe he uses from 2018 as Campana Clear. I've tested that glaze, it is fluid. (contains zinc so chrome green stains in green underglazes are going to go muddy)
-
Try some test tiles using the same glaze recipe but less of whatever type of clay is in it. I don't have the recipe for that glaze but if for example it has 25 epk in it then mix up the recipe but with 8 less epk then dip a test tile with the underglaze on it, then add 2 more epk and repeat, keep doing this until the total epk is 23 (for this example). The first test tile might craze with the epk reduced by approx 25% but there should be a tipping point where you get running from the glaze being more fluid yet not so overfluxed that it now crazes.
-
@preeta brought something up that I've been pondering for years. In this thread she asks "i wonder are potters now going to treat cobalt blue like blood diamonds? Whole ‘nother Subject." I realize as potters there's a strong probability that the cobalt we use is from the DRC and child labour plus health and safety concerns is a very valid concern in the mining practices there. We are not the reason for the mining, battery market seems to be the big driver now, but how do we feel about using cobalt or for that matter do we look into the mining practices of any of the materials we use? Cadmium inclusion stains to my knowledge are only being made in China and India, now why is that? (rhetorical question)
-
It is! I like that none of them match, well not intentionally. Opposite of how I usually work.
-
-
I bought one in January for my workroom. I like that it is voice controlled but would really recommend syncing a bluetooth speaker to it. The Echo speaker is okay for listening to the news or talk radio etc but for music I find the sound quality is pretty bad, worse when you crank up the volume. @Hulk, I don't think my wheel is ever that clean!
-
I use pretty much the same basic tools as others but also a section of a metric tape measure. I make all same type pots with lids have a standard size lid, I set the callipers to the measurement for that particular type pot or just use the tape measure. (I find metric is so much easier to measure with than imperial)
-
I lost some of the orange peel, what did go was the gray colour. (wasn't a nice gray, more of an insipid dead fish colour in parts) Like they say re-fires are a crap shoot but nothing to loose with these as I had to fix the blemishes inside.
-
Couple soda jar re-fires, there were some wadding bits from the lids that fell inside the jars that needed to be dremelled out. Touched up the glaze in the bottoms and fired them to ^6 in electric kiln. Lost a bit of the flashing colour but came out okay.
-
One of the skills I'ld like to have training in is decorative brushwork, sumi-e type work. Not necessarily black like traditional sumi-e paintings and calligraphy but I'ld love to have the skill (no small ask there!) and instruction to make fluid graceful brushwork with underglazes, stains, slips etc. edit: I realized I only answered half the question with my first reply. I would call it a trait not a skill but I can be very determined, relentless, persistent when it comes to trying to figure things out. I think this helps with sorting out the never ending ceramics related issues that arise.
-
Wish I had my own soda kiln but no,, I have the opportunity to have some pots fired in a soda kiln once in awhile.
-
This is a finished one of the oil bottles I posted a greenware photo of a few pages back, flashing slips, cone 10 soda.