    Crystalline glaze chemistry. Porcelain, Stoneware, Fritware, 04 Colored Porcelain clay research & formulation.
    Ceramics Monthly Articles: Jan. 2018 Cation Exchange (plasticity), April 2018 SSA Clay Formulation, May 2018 Bloating and Coring.
    Feb. 2019 Ceramics Monthly- Clay Body Shopping Guide
    March 2019 Ceramics Monthly - Porcelain 201
    June 2019 Ceramics Monthly Clay Restoration
    Sept. 2019 Clay Memory
    Oct. 2019 Firing Programs

    Email: optix52@aol.com

Recent Profile Visitors

34,023 profile views

glazenerd's Achievements

Advanced Member

Advanced Member (3/3)

1.8k

Reputation

Single Status Update

See all updates by glazenerd

  1. So far I am really liking 75-104 utility porcelain. I formulated it to a specific set of limits in lieu of clay varieties. I can nearly pull up a bowl almost perfectly on the first pull. I pulled up a 4" x 10" cylinder with only one pound of clay. Think I will pug out 25 lbs here shortly, interesting properties indeed.

    1. Show previous comments  2 more
    2. Joseph Fireborn

      Joseph Fireborn

      Pwning up the throwing huh?

    3. Mark C.

      Mark C.

      My supplier was out of 75-104 utility porcelain . I bought some 76-106-hope it works as good?

    4. glazenerd

      glazenerd

      I will be sending out a few trial samples in another two months or so. Currently running shrinkage and absorption tests. Shrinkage at bone dry green ware was only 3 percent.

×
×