  1. I had some Laguna ^5 Porcelain sitting around in a 5gal bucket for a year or so. Sooo, I cleaned my wheel of stoneware (spotless) and my tools, so I made some candle holders with in the Mishima technique. Do you think it would be better to fire with a clear glaze of without? I want the colors in the design to be bright.

    1. Show previous comments  4 more
    2. glazenerd

      glazenerd

      Yes you can. You will see some color shifts, pending the amount of iron in your stoneware clay. Colors will be brighter, different hues perhaps.

    3. Roberta12

      Roberta12

      again, I concur with the venerable Nerd. I go back and forth from porcelain to a white stoneware.

       

    4. Marko

      Marko

      Thank you, good people.

×
×