  1. Doing a ^6 witness firing test. I have a Orton AF3000, that is finishing at 2194 F, so I test. I have also disconnected all the switches, timers and cone sitter. Now it is direct from the elements to the power cord to the Orton control wall box. Hope it works.

    1. Mark C.

      Mark C.

      I call that seats of your pants firing and I love it. Its the way I fire most gas kilns

×
×