Back to the drawing board. I fired a kiln to ^6 with a pyro barin my sitter. New sitter, new everything, except infinite switches (no long can get), but it never got there. Brand new elements. It was firing fine till last nite. It's still cooling. Going to fire in my small kiln to finish an order. And work on the big kiln. I will fix it or try basket weaving in my padded room.
- Show previous comments 1 more
-
Yup. I just wonder if the weather had anything to do with it. We had some very heavy downpours Saturday when I was firing. No lighting. the barometric pressure was at 30.30. The humidity at 84%. Guess it could be that my kiln was, a bit under the weather, LOL.
I fired the small kiln today @^6 and it went well. Nice day. I am going to fire another load in the big kiln tomorrow ^6. small load. If it doesn't go well I am going to check all my wiring.
-
I will only fire bisque ware in my dad's big kiln. It has too many hot and cold spots. Sometimes there has been a four-cone variation between the top and bottom shelf. Too unpredictable. So I fire many small glaze loads.