Jump to content

Cavy Fire Studios

Members
  • Posts

    795
  • Joined

  • Last visited

About Cavy Fire Studios

  • Birthday 04/17/1981

Profile Information

  • Location
    A hay field in E.Washington
  • Interests
    Rodents of all kinds (GUINEA PEEGS), lagomorphs of all kinds, walruses, east Asian dragons, elephants, micaceous redart (yumyumyummy), charcoal drawing, watercolor painting, good food (Chinese!!), oldschool NES and SNES games, Chinese and Japanese ink paintings, obnoxious metal music, cute things, geeky comic book stuff, piercings and well-made tattoos.

Recent Profile Visitors

14,222 profile views

Cavy Fire Studios's Achievements

Advanced Member

Advanced Member (3/3)

322

Reputation

Single Status Update

See all updates by Cavy Fire Studios

  1. I finally got around to making an underglaze key today! Shoulda made one ages ago, honestly. With my shiny clear, what you see is NOT what you get! :)

    1. Show previous comments  2 more
    2. Chris Campbell

      Chris Campbell

      Gerstley is the worst culprit in my opinion. It does all of the above to color and also causes bleeding of colors. Find a zinc free recipe and your colors will get better immediately.

    3. Cavy Fire Studios

      Cavy Fire Studios

      Ooooh really? Huh, that's interesting. I confess I really enjoy the bleeding in my copper carb and mazerine blue, though. That might explain why Mayco's cobalt blue UG REALLY looked awful with that glaze...it makes for such beautiful bleeding effects for my shading, too. :) I think so long as my black is stable, I'm good. ♥

    4. Chris Campbell

      Chris Campbell

      As long as you know what gonna happen, you can control outcome. Just don't trust it with green! :-)

×
×