Jump to content

ChenowethArts

Members
  • Posts

    687
  • Joined

  • Last visited

About ChenowethArts

  • Birthday 01/26/1950

Contact Methods

  • Website URL
    http://www.paulchenoweth.com
  • Skype
    paul_chenoweth

Profile Information

  • Location
    Kingston Springs, Tennessee - making pots out in the woods
  • Interests
    Ceramic Musical Instruments, Figure Sculpture, Handbuilt/Thrown-altered Pieces (with music themes). Paul sketches...probably has something to do with his architectural background.

Recent Profile Visitors

20,297 profile views

ChenowethArts's Achievements

Advanced Member

Advanced Member (3/3)

471

Reputation

Single Status Update

See all updates by ChenowethArts

  1. The explosion in my bisque kiln this morning scared me so bad...'thought it was a gun shot & was just about to report it to the police.

    1. Show previous comments  3 more
    2. alabama

      alabama

      You should always pack heat when throwing, because when seconds count, police are minutes away. Sometimes you need that extra special tool just to put that unruly coffee cup or bowl out of its misery. A 22 cal. works up to 3 lbs. clay. A 38 cal. works up to 8 lbs of clay, and a 9 mm works for clay vessels over 8 lbs. of clay. My neighbors can tell the difference between a bad coffee

      cup or stein! My dogs no longer flinch!

    3. DirtRoads

      DirtRoads

      Greenware wasn't dry? I've never had an explosion ... what caused it?

    4. ChenowethArts

      ChenowethArts

      To all: It was wet greenware that exploded...kiln is fine (now that it has been emptied and thoroughly vacuumed)...still laughing at Alabama's "calibrated" recommendations :) I can only image how police would respond to the mention of "kiln"...'never really thought about it until now...there HAS to be a good joke there somewhere. -Paul

×
×