Always wanted to put raku fired items in my flower beds.  Last summer I sealed this raku fired  leaf with a gloss clear uv sealer and left it outside.

Today the snow melted so I took a picture.  Pleased to see that after being out side on the sun, rain, and freezing snow it still has the copper color.

From the album:

experimenting

  • 8 images
  • 0 comments
  • 4 image comments

Photo Information for IMG_1317.JPG experiment

Taken with Apple iPhone 5s

  • 4.2 mm
  • 1/275
  • f f/2.2
  • ISO 32
View all photo EXIF information

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.