Oatmeal and Oxblood Reduction
We borrowed our friend's light-box this weekend and went to town! This is an oatmeal and reduction red called oxblood on a heavy iron-filing filled recycled clay body. Cone 6 reduction. I am not sure about the thumb rest myself, but people seem to love it and are requesting more!