Oxblood and Oatmeal Reduction
We borrowed our friend's light-box this weekend and went to town! This is an oatmeal and reduction red called oxblood on a heavy iron-filing filled recycled clay body. Cone 6 reduction. Wonky handles as these are the first batch of mugs I made a few weeks ago. I have since learned a better technique!