Eucalyptus Grove Platter
This is my very first platter or plate of any kind, although I have made a few pie plates.
I actually intended this to be a pie plate but accidentally "stepped on the gas" just as I was finishing so the walls spun out almost flat. I decided it was a platter instead. I'm very happy with how this turned out.
White stoneware, thrown on the pottery wheel, carved in a design of eucalyptus leaves in the wind. Glazed in Mayco's Stoned Denim at ^6 in an electric kiln. (Actually fired twice because the first time a cookie exploded and got shards everywhere.)
Copyright
© Giselle No. 5 Ceramics 2016, all rights reserved