Slate Blue Carved Mountain Tumbler
Thrown on the pottery wheel in white stoneware, carved deeply with mountain design. Treated with 2-1 water and iron oxide mix on only the mountains. One coat Mayco's Stoned Denim on mountains, four coats on everything else. Fired at ^6 in an electric kiln.