Hydria Work-in-Progress
Upper parts of the hydria are starting to come together. The container is just over 18" tall at this stage and was wheel thrown in two parts, assembled on the wheel, allowed to dry for a few hours and then given the final shaping/neck-forming. With the addition of the footed-base, the greenware will stand just under 24" tall...that cannon happen until the base is hardened sufficiently to hold the weight of the upper portions.