It looks like it is back to square one on this project. Attachments to this piece created some sizable air pockets that I did not pierce with a needle to allow air to escape...so, it didn't, and this is the result. It is quite a mess. Thankfully, it is not a mistake that I make often.

Copyright

© Copyright 2015, Paul M. Chenoweth, Nashville, TN USA. All rights reserved.
From the album:

Tornado Pot Sketches and Progress Images

  • 15 images
  • 0 comments
  • 40 image comments

Photo Information for Not Everything Turns Out As Planned

Taken with Canon Canon PowerShot G16

  • 6.1 mm
  • 1/60
  • f f/1.8
  • ISO 400
View all photo EXIF information
 Share


Recommended Comments

This is my mistake, Guinea...'completely preventable had I not been in a hurry (or having a 'senior' moment).  The pieces have been retired (trashed) and the kiln is all vacuumed out and ready to roll.

:)

Link to comment

Shame! It is such a helpless feeling..... AND knowing it could have been prevented!! Well, we never get too old to learn and to be reminded of things that we already know and practice...... patience, my dear Watson, patience....

Susan

Link to comment

SusanL... So true. Even an old dog can repeat silly mistakes (or something like that) :)
 
"The key to everything is patience. You get the chicken by hatching the egg, not by smashing it."
-Arnold H. Glasow

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.