Jump to content

Cone 9 Celedon Glaze


Marcia Selsor

Celedon ^9 reduction using burnt umber for a colorant.This was the color I wanted for ^6 Ox.

I did many tests and came up with the recipe posted in the previous Faux celedon example.

From the album:

forum discussions

· 17 images
  • 17 images
  • 0 comments