Porcelain

Cone 6, multiple firings

 

 

I saw a video on double walled pots and thought that it looked like a lot of fun so I thought I'd give it a whirl. I did some searches on etsy and youtube to see what people made and for the most part I was unimpressed. Most were too thick and chunky and the carving was geometric and kinda boring, I figured I could learn from their mistakes.

 

I love lotus flowers so I decided to do this kinda underwater scene. I wanted to play with the different elemnets that are provided, so placing the carved fish as a kind of middle ground would strengthen the foreground and background.

Sign in to follow this  
From the album:

Sample Work

  • 10 images
  • 0 comments
  • 6 image comments

Photo Information for My 1st atempt at a double walled teapot


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.