Ready for glaze fire.

The depth bit on the caliper is handy for poking out the teapot lid's breathing hole.
Do you blow out the hole the first time (liner glaze)?
How about the teapot spout? Do you blow out the excess as part of the liner glaze step?

The ketchup squirter is handy for several glazing jobs.
...yep, the tape label reads "Min IV" - it's my liner glaze, a whiteish clear.
In my journey toward a well-fitting liner - crazing was the main problem - I'd started over with a new recipe.
The name reflects the original recipe's source. Thanks Min.
The proportions have been adjusted four times.
It's not too soon to start on "next" - for my Petalite supply is running low...

Taping the foot ring gives me a clean line, and, AND a finger hold for pushing the ware upside down into the glaze.
Removing the tape (low over the trash can, so the bits all fall in), last thing before setting the ware down after dipping, is just right, for the glaze isn't dry enough to dust up.


From the album:

Studio

· 8 images
  • 8 images
  • 0 comments
  • 5 image comments

Photo Information


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.