Jump to content

Feldspar Potash - Odd Colours


Chilly

Recommended Posts

I have a bucket of Feldspar Potash that is wet.  It is creamy coloured on the top of the bucket (with green mould right on the top), then grey with red staining throughout the rest of the bucket.

 

I nearly threw it out thinking it was contaminated with something else.  But....

 

On drying it out, it has all reverted to the creamy colour!

 

Can anyone explain this please?

post-59202-0-92980400-1409086447_thumb.jpg

post-59202-0-24854500-1409086457_thumb.jpg

post-59202-0-62820600-1409086458_thumb.jpg

post-59202-0-92980400-1409086447_thumb.jpg

post-59202-0-24854500-1409086457_thumb.jpg

post-59202-0-62820600-1409086458_thumb.jpg

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.