PeterH Posted April 8, 2014 Report Share Posted April 8, 2014 Has anyone out there successfully done sugar raku? If so, can you tell me what post-firing treatment you used, and what the results looked like. I've tried several times using the usual smoke/reduction bin (as for naked raku), and got a very dark two-tone grey. This sounds like it could be subtle and sophisticated, but wasn't. Regards, Peter Link to comment Share on other sites More sharing options...
DarrellVanDrooly Posted April 9, 2014 Report Share Posted April 9, 2014 When I do horsehair firings, I sprinkle sugar on the pots. The sugar leaves a black mark where every grain hit the pot. It is quite pretty. I rub my pots in coconut oil post firing to alter the color slightly and make it slightly more smooth. Other potters I know use tile sealer on their pots to make 'em all shiny. (this is fired to ^012, removed from the kiln while hot and have had granular sugar thrown at them.) Link to comment Share on other sites More sharing options...
Graeme Posted April 9, 2014 Report Share Posted April 9, 2014 Peter. I've never used sugar in raku. Perhaps you are thinking of black firing, where sugar is thrown into the kiln at the top temperature, and the kiln tightly sealed. Any gaps allowing air to enter will result in grey patches. Cheers. Graeme. . Link to comment Share on other sites More sharing options...
PeterH Posted April 14, 2014 Author Report Share Posted April 14, 2014 Thanks, but the sugar raku I'm interested in is a variant of the 2-part naked raku process, inwhich the refractory 1st coat contains sugar. Normally 2-part naked raku leaves black "crackle"lines. On the other hand sugar raku -- from the few photos I've seen -- leaves black patches,often with some sort of halo effect. Overall effect is something like the left-hand pot in http://tinyurl.com/pzubofy Every few years I'd try again using the normal 2-part naked raku process, and got a really ugly pot in a mixture of black and charcoal greys. Last time I tried cooling it in oxidation, with more interesting results. Firstly tried quenching as soon as it came out of the kiln. Then letting it air cool sitting on a brick Different, but nothing like the pictures I'd seen. Finally I tried to repeat the second experiment, but botched it. I put it on short damp grass to cool, and it had fallen on its side by the time I got back. Obviously it had seen a mixture of oxidation and reduction. So, I'm interested to know how other people cool their sugar raku. Regards, Peter For completeness. Fired somewhere in the range 1030-1050C. Slip was china clay 3, flint 2, sugar 2 by volume. I also tried a 3:2:1 mix but it was rather faint. Link to comment Share on other sites More sharing options...
Tyler Miller Posted April 15, 2014 Report Share Posted April 15, 2014 Peter, I'm not entirely convinced that the example photo you've posted there is a product of sugar raku alone, or maybe at all. I think those pots are Geoffrey Swindell's work: http://www.geoffreyswindellceramics.co.uk/ Maybe drop him a message and see what he thinks? I think the results you've got are something. The only bad result would be if nothing showed up at all, since that's the only result you couldn't have learned from (aside from complete success). Do you keep a firing log? They're very helpful in figuring things out over time. If you're committed to mastering this technique, I would start by recording everything you do every time you attempt it, right down to an accidental sneeze you made over your kiln during firing. Play with variables, one variable at a time. You've decreased sugar, now increase it. Play with the slip resist recipes you use. What does it look like when the sugar isn't fully dissolved or the solution is super saturated? What about when it's completely dissolved? In my experience with ceramics, doing exactly what one potter does, especially with raku, doesn't mean you'll get that potter's result. Link to comment Share on other sites More sharing options...
Evelyne Schoenmann Posted April 15, 2014 Report Share Posted April 15, 2014 Here in Europe the couple Ed + Ine Knops are famous for their great Raku knowledge. Maybe you could send an email to Ed, asking him whether he knows something about sugar Raku?! ed@knopsclay.demon.nl Greetings Evelyne Link to comment Share on other sites More sharing options...
Idaho Potter Posted April 17, 2014 Report Share Posted April 17, 2014 I work with raku a lot, and the third picture is dazzling--in my opinion. I've never tried or heard of sugar raku, but I would be happy with the pot in picture #2, and overjoyed with the outcome in #3. Shirley Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.