Jump to content
Sign in to follow this  
Mark C.

Favorite Glaze Tools-Squeeze Bottles-Brushes-Pourers

Recommended Posts

The string on squeeze bottles got me thinking so as today was Friday which has been my third Friday in a row glazing a kiln load-after cleaning up and loading I gathered some- not all of my fav-glazing tools-

I like all sizes of bottles and brushes-these are all ones I made from my bamboo and mostly skunk and elk hair-the smaller bushes I use are commerical ones. I hang them all when not in use.

The glaze pourers are thru amazon -they have long necks the small one is two cups the large is 3 /12cups-I think they are batter pitcher's.

You can control where you want glaze with this tool when pouring.

When you have a car kiln a week to glaze up in a day you need to be quick and dipping and pouring are fast. I also do a lot of squeeze bottle and brush work.

This was a big work push that ends with a long drive to a show next week.

Mark

 

post-8914-0-53511000-1395452808_thumb.jpg

post-8914-0-97847100-1395452817_thumb.jpg

post-8914-0-18963200-1395452832_thumb.jpg

post-8914-0-53511000-1395452808_thumb.jpg

post-8914-0-97847100-1395452817_thumb.jpg

post-8914-0-18963200-1395452832_thumb.jpg

Share this post


Link to post
Share on other sites

Envious of those brushes Mark.

Will go looking for those long snouted beakers.

So you don't store slip in those bottles between glazings?

Bettert  take some of those trolley images to Hawaii

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.