Chris,

 

Grog is pretty cheap to buy.... no real economic savings in making your own. ;)

 

best,

 

..................john


John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#82 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,179 posts
  • LocationCentral, PA

Posted 10 February 2014 - 09:52 AM

Looking at your shards and survivors, I would make a few personal observations. Your quest for answers told you that cold ware that feels damp will have ice in the clay that will hide its amount of wetness, also causing extremes when fired.  Secondly I would think you would want the walls of the "rocks" thinner in order to be flottable.  The survivors look good, and it would be interesting to see the finished pieces.  As I have stated before, I once ran a project with slab construction that used  large river stones (5-8#) as forms the students would roll out 3/8" slabs and wrap completely, paddle to smooth, cut in half on a bevel when leather hard and rejoin. You might try the same.


Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#83 Norm Stuart

Norm Stuart

    Advanced Member

  • Members
  • PipPipPip
  • 639 posts

Posted 10 February 2014 - 02:32 PM

Chris Campbell and I have a challenge to see which of us can fire the thickest greenware.

 

I have various solid clay blocks drying currently, some up to 3 inches thick, with a new custom bisque schedule to fire them.

 

Alexandre Bigot experimented with very slow-firing kilns for architectural sized ceramics before he switched over to using hydraulic presses to form pieces with grog and other material which did not off-gas.

 

Regardless of how slow you fire, there is an absolute maximum thickness you can fire with each clay before developing cracks.

 

Looking at your shards and survivors, I would make a few personal observations. Your quest for answers told you that cold ware that feels damp will have ice in the clay that will hide its amount of wetness, also causing extremes when fired.  Secondly I would think you would want the walls of the "rocks" thinner in order to be flottable.  The survivors look good, and it would be interesting to see the finished pieces.  As I have stated before, I once ran a project with slab construction that used  large river stones (5-8#) as forms the students would roll out 3/8" slabs and wrap completely, paddle to smooth, cut in half on a bevel when leather hard and rejoin. You might try the same.



#84 Pres

Pres

    Retired Art Teacher

  • Moderators
  • 3,179 posts
  • LocationCentral, PA

Posted 10 February 2014 - 02:36 PM

Oh, I thought she was into creating floating rocks as are used in some Chinese water gardens?  My mistake.  However, if the clay in her shop is near freezing, it certainly put her at a disadvantage.


Simply retired teacher, not dead, living the dream. on and on and. . . . on. . . . http://picworkspottery.blogspot.com/

#85 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,265 posts
  • LocationWilton, NH USA

Posted 10 February 2014 - 06:45 PM

Look at Jun Kanako's works.

 

best,

 

.............................john


John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#86 Norm Stuart

Norm Stuart

    Advanced Member

  • Members
  • PipPipPip
  • 639 posts

Posted 11 February 2014 - 12:03 AM

John -- Anything you wold change with my "thick pieces bisque" before I use it next week?

 

                   F/Hr     F      Hold

1  RAMP        60      200   8 hours

RAMP      100      350

3  RAMP      350      950

4  RAMP      100    1,000          

5  RAMP        50     1,150

6  RAMP      400    1,638                           

7  RAMP       108     1,888   30 Minutes

8  RAMP      400     1,100

9  RAMP      200     1,400

 

Look at Jun Kanako's works.

 

best,

 

.............................john



#87 Babs

Babs

    Advanced Member

  • Members
  • PipPipPip
  • 2,076 posts

Posted 11 February 2014 - 01:23 AM

Oh, I thought she was into creating floating rocks as are used in some Chinese water gardens?  My mistake.  However, if the clay in her shop is near freezing, it certainly put her at a disadvantage.

I think she is BUT what I've read of Chris she is prob immersed in about 90  ceramic projects, cooking for 40, knitting for charity and washing the cat! All before Breakfast, and smiling!

AND willing to fail better in every one of these ideas.

Chris these are the Scottish potters stones from her Book Floating stones.

Pres, you can see the thickness she uses and they are thinner than Chris's

Artist's name is actually Lotte Glob , my misspelling