Posted 26 June 2013 - 08:43 AM

I need to buy some new kiln shelves and I am considering lighter shelving. I do not need a whole new set just some additions, but I am concerned that firing with two different kinds of shelves will cause uneven heating because of different heat absorption. Is there any good reason to stick to the same shelving I already have or can I mix it up?

Thanks!

Julia

juliapaulpottery.com


#2 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 26 June 2013 - 08:51 AM

Julia;
You don't say what temperature you are firing to. Also, are you firing electric or gas?Reduction,oxidation?
TJR.

#3 Arnold Howard

Arnold Howard

    Graduate, School of Life

  • Members
  • PipPipPip
  • 268 posts
  • LocationMesquite, Texas USA

Posted 26 June 2013 - 08:57 AM

I need to buy some new kiln shelves and I am considering lighter shelving. I do not need a whole new set just some additions, but I am concerned that firing with two different kinds of shelves will cause uneven heating because of different heat absorption. Is there any good reason to stick to the same shelving I already have or can I mix it up?


Julia, that is a good question. It is okay to fire shelves of different types in the same kiln. If a thinner shelf needs more thermal density so that it matches the other shelves, just load more mass on that thinner shelf.

If you are making production ware and have developed a precise loading pattern, where each shelf has a set number of pieces and is placed in the same part of the kiln for every firing, then a different shelf type may
disturb your loading plan. Otherwise it won't matter.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
[email protected] / www.paragonweb.com

#4 Min

Min

    Advanced Member

  • Members
  • PipPipPip
  • 1,485 posts
  • LocationCanada

Posted 26 June 2013 - 10:42 AM

I usually use 5 shelves in my front loading kiln, acme marls. I picked up 2 Corelite shelves to try out. Haven't noticed any difference in the firings, I use the Corelite for the top 2 shelves since those are the ones I have to lift the furthest. I'm a shorty and my back appreciates the lighter shelves. ^7 electric

Min

#5 jpclay

jpclay

    Newbie

  • Members
  • Pip
  • 7 posts
  • LocationVirginia

Posted 26 June 2013 - 12:39 PM

Thank you for the responses. I am firing in an electric to cone 6. I am not doing production, so I have some flexibility, but I also do not want to have to be fussy and adjust the loading because I have different shelves.

Julia

juliapaulpottery.com


#6 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,228 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 26 June 2013 - 03:05 PM

The thinest and lightest are advancers by far
The cheaper other option is the hollow corelites
Mark
Mark Cortright
www.liscomhillpottery.com

#7 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,995 posts
  • LocationGrayslake, IL

Posted 26 June 2013 - 05:19 PM

I love my CoreLites!

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users