Posted 01 September 2010 - 03:12 PM

What is an ideal bisque temperature for raku clay before raku glazing? Will bisque firing temperature will have effect on results of Raku glaze? please help.

#2 ~janie

~janie

    ~janie

  • Members
  • PipPipPip
  • 103 posts
  • LocationHot old Texas Coast

Posted 01 September 2010 - 05:32 PM

What is an ideal bisque temperature for raku clay before raku glazing? Will bisque firing temperature will have effect on results of Raku glaze? please help.


I am not the most experienced person to be teaching anyone, but I will share what I have been taught.

Bisque is bisque, regardless of the clay. Clay is formed, dried and dried, then fired to bisque, usually between 1700-1800 degrees, although we fire a bit higher, at cone 06. The point where clay becomes ceramic (the ceramic change) occurs at 1112 degrees, however.

I cannot imagine that the bisque temperature would affect your raku glaze. It will only be affected by what you do after you put the glaze on your piece. We fire all our raku at cone 06- 1830 degrees, and use glazes formulated for that temperature.

If I have got this backwards, I would appreciate being set straight, too.

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,328 posts
  • LocationRed Lodge, Montana

Posted 01 September 2010 - 05:42 PM

I agree.I bisque anywhere from ^06 to ^04 for Raku.
I like to take my slabs a little hotter than the Raku firing just for extra strength.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Potterstu

Potterstu

    Member

  • Members
  • PipPip
  • 15 posts
  • LocationSouthern Arizona

Posted 02 September 2010 - 12:47 PM

I bisque at C/04 and fire raku at 07 to 06. This helps in two ways. I agree with Marcia that bisquing higher than the final firing helps ensure strength, and I sometmes like to burnish my clay and by firing cooler than bisque, I don't loose the burnish.

Stuart


#5 Kiln-man

Kiln-man

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 13 September 2010 - 04:13 PM

What is an ideal bisque temperature for raku clay before raku glazing? Will bisque firing temperature will have effect on results of Raku glaze? please help.


The ^06 to ^04 is what I have seen most people use. The only restriction is the clay body temperature.
Do not exceed it.

#6 Deb Evans

Deb Evans

    Advanced Member

  • Members
  • PipPipPip
  • 98 posts
  • LocationBlue Mtn Lake, NY

Posted 21 September 2010 - 11:50 PM

I always found ^ 04 bisque was sturdier for fragile pots (tongs can break soft bisque), than glazes were for ^05,06 firing