Posted 19 March 2013 - 02:44 PM

Does anyone know if it is bad to layer a clear (sahara) amoco glaze over a coyote satin finish glaze? I have the colors I need but I am pretty sure the person wanting the item (fruit bowl) wants glossy.

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 19 March 2013 - 03:04 PM

Putting a clear glaze over a satin glaze will not just gloss up the satin. They will blend and alter both glazes, essentially creating a third glaze. It doesn't work like underglazes, which don't melt and blend with the clear glaze.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 Rebekah Krieger

Rebekah Krieger

    The extraordinary clay bender

  • Members
  • PipPipPip
  • 786 posts
  • LocationWisconsin

Posted 19 March 2013 - 05:51 PM

Putting a clear glaze over a satin glaze will not just gloss up the satin. They will blend and alter both glazes, essentially creating a third glaze. It doesn't work like underglazes, which don't melt and blend with the clear glaze.


Thanks for answering another one of my questions :D

~ Namaste ~

 

Home studio potter 

 

Shanel Pottery 

www.shanelpottery.com

www.facebook.com/shanelspottery 

 

 

 

"To me the greatest thing is to live beauty in our daily life and to crowd every moment with things of beauty.  It is then, and then only that  the art of the people as a whole is endowed with it's richest significance.  For it's products are those made by great a many craftsmen for the mass of the people, and the moment this art declines the life of the nation  is removed far away from beauty.  So long as beauty abides in only in a few articles created by a few geniuses, the kingdom of beauty is nowhere near realization."                                                                                 - Bernard Leach 

#4 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 21 March 2013 - 12:33 AM

Mixing glazes is NOT a matter of A+B=C.... Sometimes A+B=Q... I use a nice transparent blue-green glaze I buy by the pint. I found if I put it over a white glaze, it produces a beautiful roiling blue and white, but it totally looses the green.

In other words, you won't really know what you're going to get until you do a trial.
Maryjane Carlson

Whistling Fish Pottery

#5 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 21 March 2013 - 09:15 AM

Mixing glazes is NOT a matter of A+B=C.... Sometimes A+B=Q... I use a nice transparent blue-green glaze I buy by the pint. I found if I put it over a white glaze, it produces a beautiful roiling blue and white, but it totally looses the green.

In other words, you won't really know what you're going to get until you do a trial.


Very good analogy. I always tell my students, glazes are not paint. Mixing blue and yellow, might give you green. But it could also give you pink.....I've never had that happen, with my glazes, but I think it illustrates the point.

.....Because of this discussion, I'm half way tempted to go and make some test tiles, with clear layered over top each of my other glazes.....