Hi All,

 

I want to use a white slip over a dark brown body. I have a white clay in mind, to make the slip, that has the same shrinkage rate but different absorption rate (2.7 for the body vs. 1.2 for the slip). Will the difference cause any issues?

 

Thanks, Mark