Ok....... here's a "monochromatic assignment" for you all to chew on..........

If you could only use one colorant in your work....what would you choose and why?



Check out joining the Potters Council ( www.potterscouncil.org ) for more networking possibilities, peer mentoring opportunities, discounts on books, magazines, and DVDs, health insurance, credit card merchant programs, and many other member benefits.

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore


#2 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 11 January 2013 - 11:03 AM

Copper Carbonate. Rich color variation just by using different amounts. Greens and blues in oxidation, red in reduction.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,330 posts
  • LocationRed Lodge, Montana

Posted 11 January 2013 - 12:15 PM

Copper because it can go red, turquoise, blues, and greens in Oxidation and Reduction depending on the base chemistry.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Lucille Oka

Lucille Oka

    Advanced Member

  • Members
  • PipPipPip
  • 756 posts
  • LocationCalifornia

Posted 11 January 2013 - 03:33 PM

Cobalt, because it is my favorite colorant, it is dependable, the most beautiful and a little goes a long way. I always make sure I have a variety of cobalt compounds available.


John 3:16
"For God so loved the world that He gave His only begotten Son, that whosoever believeth in Him should not perish but have everlasting life".

#5 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,304 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 11 January 2013 - 03:33 PM

Copper for all the same reasons.
35 years ago it was Iron now its copper.
Mark
Mark Cortright
www.liscomhillpottery.com

#6 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,330 posts
  • LocationRed Lodge, Montana

Posted 11 January 2013 - 11:03 PM

I thought about the wide variety of iron too.But I " chose wisely " and picked copper.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#7 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 12 January 2013 - 07:26 AM

I say cobalt carb., because it is beautiful, always shows up, unlike copper, and everyone loves it. I am talking about a small amount as on-glaze decoration, not a blue glaze.
TJR.

#8 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 12 January 2013 - 09:52 AM

I thought about the wide variety of iron too.But I " chose wisely " and picked copper.

Marcia


Me, too. The subtle beauty of a celadon and the striking beauty of a golden iron saturate are hard to beat.