      Ceramic Arts Network is looking for two new forum moderators for the Clay and Glaze Chemistry and Equipment Use and Repair sections of the Ceramic Arts Network Community Forum. We are looking for somebody who is an active participant (i.e. somebody who participates on a daily basis, or near daily) on the forum. Moderators must be willing to monitor the forum on a daily basis to remove spam, make sure members are adhering to the Forum Terms of Use, and make sure posts are in the appropriate categories. In addition to moderating their primary sections, Moderators must work as a team with other moderators to monitor the areas of the forum that do not have dedicated moderators (Educational Approaches and Resources, Aesthetic Approaches and Philosophy, etc.). Moderators must have a solid understanding of the area of the forum they are going to moderate (i.e. the Clay and Glaze Chemistry moderator must be somebody who mixes, tests, and has a decent understanding of materials). Moderators must be diplomatic communicators, be receptive to others’ ideas, and be able to see things from multiple perspectives. This is a volunteer position that comes with an honorary annual ICAN Gold membership. If you are interested, please send an email outlining your experience and qualifications to jharnetty@ceramics.org.
Sign in to follow this  
Hermes

Recording Ceramic Parameters - Part I

Recommended Posts

Keeping record of your work

 

 

In literature it is often mentioned to keep record of all details of the ceramic work pieces. This is not a superfluous recommendation. It is the only way to progress and improve the quality of ones creations. On top, if you are interested in the chemistry of glazes like me, one can gather an impressive quantity of data that allows to understand better and better how complex glaze chemistry can be and,... it is fun!

 

What to keep record of? Everything! There is no limit! Even to some extend, recording weather conditions can be of importance. Not that I am going that far...

 

The minimum tool is a good notebook, kept in good order. Although this can be a sufficient tool, modern technology helps us to do it in an elegant and in a visually rich way.

 

The main tools I use are INSIGHT for easy glaze calculation (this -or similar- can already be used as a good recording database) .

 

I use Excel for making graphs of:

 

· A firing diagram

 

· Alumina/Silica ratio plots

 

· Ternary graphs of Mole% of Fluxes, Amphoteric and Glass formers

 

· Limit bar graphs based on the Unity formula

 

· Comparative graphs of glazes with different thermal expansion

 

All of the above are combined in a Filemaker database.

 

As an example here is a picture of a firing diagram. It contains besides the temperature also the gas pressure and the damper opening during the firing.

 

In a forthcoming post I will show some more examples of how it may look.

 

firing%20diag.jpg

 

 

 

 

 

Find more about ceramics on my web pages:

http://users.telenet...Spruyt/Ceramics menu.html

Share this post


Link to post
Share on other sites

Hermes:

 

Thank you for taking the time to post these. I've enjoyed both of the ones that I have read. As a newby, I'm constantly amazed at how helpful all of you on the forum are!

Share this post


Link to post
Share on other sites

One thing I've started doing is taking a pic of a piece that I'm doing something extra too (verses production ware), and numbering it, and then jotting that number in my notebook along with relevant data. Later I can transfer the pic from my phone to my computer.

 

Joel.

Share this post


Link to post
Share on other sites

Hermes:

 

Thank you for taking the time to post these. I've enjoyed both of the ones that I have read. As a newby, I'm constantly amazed at how helpful all of you on the forum are!

 

 

Thank you for your interest

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.