Thanks Chris, for the suggestions.

I do have the manual for the kliln, I had not used the cone fire function because it does not have a hold at peak temp, I had been told by Skutt that I needed to hold for 10-15 min at 2200 for more even firing.

I have also talked to a man at a large S East show with beautiful cone6 elec glazes that said, "Lady,just hit ^6 and START and go back to the house".

 

 

My KilnMaster II on my new (this summer) Skutt 1018 allows holds in the cone fire mode. Check the manual again. In the Cone fire mode, after entering the preheat, the cone number, then the speed, there should be a hold prompt.

 

Good luck.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.