GA_Clayman67 Posted December 2, 2012 Report Share Posted December 2, 2012 Back into the clay after 37-years away and I'm having what has to be a simple problem, but I'm flummoxed! Making very basic business card holders from slabs. I'm draping the cut piece of clay over a plastic covered 2x4 and letting it sit for 24-hours - also covered. Then, removing the plastic and allowing the pieces to dry on the 2x4. My problem: nearly all the pieces are cracked after the second day and unusable. What can I do to prevent this? Many thanks in advance! Art Carlson Link to comment Share on other sites More sharing options...
bciskepottery Posted December 2, 2012 Report Share Posted December 2, 2012 Your clay is shrinking against the rigid form. You need to remove them from the form sooner and be allowed to dry on their own. Link to comment Share on other sites More sharing options...
GA_Clayman67 Posted December 2, 2012 Author Report Share Posted December 2, 2012 Your clay is shrinking against the rigid form. You need to remove them from the form sooner and be allowed to dry on their own. Thanks - makes perfect sense. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 2, 2012 Report Share Posted December 2, 2012 Or you could work within a negative right angle. When using wood forms, try sprinkling bal clay or corn starch on the surface to eliminate the clay from sticking to a rigid form. I use newsprint paper between clay and forms when necessary. The link is definitely overkill for business card size, but you will get the idea. http://ceramicartsdaily.org/clay-tools/making-clay-tools/the-right-angle-for-approaching-geometric-ceramic-sculpture/ Marcia Link to comment Share on other sites More sharing options...
GA_Clayman67 Posted December 2, 2012 Author Report Share Posted December 2, 2012 Or you could work within a negative right angle. When using wood forms, try sprinkling bal clay or corn starch on the surface to eliminate the clay from sticking to a rigid form. I use newsprint paper between clay and forms when necessary. The link is definitely overkill for business card size, but you will get the idea. http://ceramicartsda...amic-sculpture/ Marcia Thank you! I like the idea of corn starch - will try that next time around. Link to comment Share on other sites More sharing options...
weeble Posted December 3, 2012 Report Share Posted December 3, 2012 IF you're draping around two corners, it won't work because the clay is shrinking as it dries and the board is not. If just around one corner, you could get away with putting something between the form and the clay so its not stuck to the form as it dries. My current go-to favorite is an old paper towel, but if I'm drying slowly a piece of saran wrap works just fine as long as I cover both sides Link to comment Share on other sites More sharing options...
GA_Clayman67 Posted December 5, 2012 Author Report Share Posted December 5, 2012 IF you're draping around two corners, it won't work because the clay is shrinking as it dries and the board is not. If just around one corner, you could get away with putting something between the form and the clay so its not stuck to the form as it dries. My current go-to favorite is an old paper towel, but if I'm drying slowly a piece of saran wrap works just fine as long as I cover both sides Maryjane... thanks... Saran Wrap's a real pain - delighted to hear a paper towel works as well! Link to comment Share on other sites More sharing options...
weeble Posted December 6, 2012 Report Share Posted December 6, 2012 Yep, just be sure to get CHEAP paper towels... I ran into some of the spendy ones that have some sort of softener in the paper that actually left marks on the fired piece. VERY strange, almost like a series of very fine wax resist dots anywhere they were in contact with the clay, even after the bisque. Would have been great if that was what I was looking for, but they wouldn't take the terra sig I was TRYING to apply. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.