I'm fairly new to slab work. Any suggestions for cleaner edges would be appreciated. I'm working with Buncombe White and Highwater P-5 porcelain, both ^5-6.


"Saving just one dog won't change the world, but it surely will change the world for that one dog."


#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,066 posts
  • LocationRaleigh, NC

Posted 16 July 2010 - 09:09 AM

I don't really understand your question ...
At what stage you having the problem?

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 Pam S

Pam S

    Advanced Member

  • Members
  • PipPipPip
  • 160 posts
  • LocationDurham, NC

Posted 16 July 2010 - 10:41 AM

For example, the exposed edges of a slab built box. The edges alway look a little ratty to me. I've tried compressing them slightly with a sponge and a chamios but they never have that smooth finish that a wheel thrown piece has. Thanks.


"Saving just one dog won't change the world, but it surely will change the world for that one dog."


#4 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,066 posts
  • LocationRaleigh, NC

Posted 16 July 2010 - 05:23 PM

One trick for smooth edges is to put dry cleaner plastic over the cut pieces ...
smooth the edges by running your fingers over them through the plastic.

Doesn't stick that way and the plastic really helps compress those edges.

You can also cut the pieces out through the plastic by pressing down rather
than slicing through ... Make sense?

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#5 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,671 posts
  • LocationNorthern Virginia

Posted 16 July 2010 - 07:31 PM

For example, the exposed edges of a slab built box. The edges alway look a little ratty to me. I've tried compressing them slightly with a sponge and a chamios but they never have that smooth finish that a wheel thrown piece has. Thanks.




I use a chamfer tool -- sold by Bill Van Gilder -- to clean exposed edges of slabs. The tool, which he adapted from those used by woodworkers, allows me to put a nice bevelled finish on edges at the leatherhard stage. I also use Buncombe White; the clay has kyanite in it and if you use a wet sponge you run the risk of exposing the grit in the clay because the sponge washes away the finer clay particles. A soft rib can give you a smooth look and help compress the edge or seam.

#6 Pam S

Pam S

    Advanced Member

  • Members
  • PipPipPip
  • 160 posts
  • LocationDurham, NC

Posted 16 July 2010 - 09:57 PM

Both suggestions make sense! I'll try both. Dry cleaners plastic first since I have plenty! I have noticed the exposure of grit when using a sponge on the Buncombe White. From the two responses, I think I've also been getting a bit ahead of myself in trying to smooth the edges. I've been trying to achieve this while the clay is very damp. Perhaps if I wait...

"Saving just one dog won't change the world, but it surely will change the world for that one dog."


#7 AndyL

AndyL

    Advanced Member

  • Members
  • PipPipPip
  • 165 posts
  • LocationNJ, USA

Posted 16 July 2010 - 10:50 PM

You could let the slabs stiffen up to cheesehard by putting them in the sun. BTW a cleaner edge for assemblies like boxes can be made with a bevel tool. I use 45º and 30º/60º bevel cutters.

#8 Pam S

Pam S

    Advanced Member

  • Members
  • PipPipPip
  • 160 posts
  • LocationDurham, NC

Posted 17 July 2010 - 03:59 PM

I used Chris' method with dry cleaning plastic today on stiff but not leather hard clay. Worked like a charm! I can't wait to try cutting the clay with the plastic! Many thanks!!!

"Saving just one dog won't change the world, but it surely will change the world for that one dog."


#9 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,139 posts
  • LocationRed Lodge, Montana

Posted 18 July 2010 - 10:39 AM

For a crisp edge I use a sur-form tool.
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#10 charles varni

charles varni

    Newbie

  • Members
  • Pip
  • 2 posts
  • LocationOceano, California

Posted 19 July 2010 - 08:03 AM

I'm fairly new to slab work. Any suggestions for cleaner edges would be appreciated. I'm working with Buncombe White and Highwater P-5 porcelain, both ^5-6.



When your piece is leather hard use a "sureform" rasp to shave the edges straight, curved or whatever. Then smooth with damp sponge. I use the small curved sureform.