AndyL Posted October 22, 2012 Report Share Posted October 22, 2012 I was thinking of experimentally saggar firing in my electric kiln at ^016. I was considering doing this in a 10 gallon galvinized trash can. The kiln has a electric ventilator that'll be on as it fires. Opinions on these thoughts appreciated. Link to comment Share on other sites More sharing options...
Mark McCombs Posted October 23, 2012 Report Share Posted October 23, 2012 I think that Zinc has a pretty low melting point 700 - 800 degrees F. Not sure how that would work out. Sounds kinda messy. Link to comment Share on other sites More sharing options...
dave the potter Posted October 23, 2012 Report Share Posted October 23, 2012 zinc fumes are really dangerous and occur at low temperatures. This is infinitely more dangerous than dust from fiber blanket Link to comment Share on other sites More sharing options...
neilestrick Posted October 23, 2012 Report Share Posted October 23, 2012 Better to either make a clay saggar, or build one out of kiln bricks. The fumes from the galvanized are dangerous, and the can probably won't hold up well anyway. Link to comment Share on other sites More sharing options...
ClayByMck Posted December 3, 2012 Report Share Posted December 3, 2012 This is my fav way to put that can to good use. Fill the can with paper, straw, etc and put it aside. Roll out an eighth inch slab and start sticking stuff to it, like salt water soaked leaves, crushed pine cones, rock salt, cobalt carb, copper, steel wool, u get the gist. After that treasure hunt I take my prepared piece of pottery (usually with tera sig, and so on) and wrap the littered slab completely around it. Throw it in the kiln and ramp that baby up to 1300ish 1400ish. Pull it out red hot and toss it shell and all into that trash can u love so much and let it burst into flames for a few seconds before placing the lid on tight. Let it reduce with the lid on for at least 30 minutes. When your ready to be amazed, pluck it from the can, pull away what's left of the eighth inch shell and admire its beauty. Thow a coat of wax on it if u like. Its kinda an electric saggar salt raku kinda thing and you'll love it. Remember to always play with fire responsibly and good luck. Link to comment Share on other sites More sharing options...
weeble Posted December 3, 2012 Report Share Posted December 3, 2012 I've managed to do some pretty serious damage to trash cans with just lighting a fire inside, I suspect putting one in a kiln would be a one-time-only mistake. As in, that would be the one last time you use the kiln.... In other words, find a different saggar.... Link to comment Share on other sites More sharing options...
Judd Posted December 11, 2012 Report Share Posted December 11, 2012 A potter friend of mine said he'd get those metal tin cans you get popcorn during Xmas. He said he filled it with sawdust, greenware, salt, steel wool, whatever, more sawdust, the lid then a kiln shelf on top to hold in all the smoke and trash. He'd put it in his electric kiln and fire around 1100, then let it cool to room temp. He said the cans warped, but the smoke didn't get out and ruin the elements. *Please note: I think my friend may be a crazy crack-head. Not sure I'd try this in my kiln. Still sounds cool. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 11, 2012 Report Share Posted December 11, 2012 Here is the website of Russel Fouts who has published several articles on saggar firing in electric kilns http://users.skynet.be/russel.fouts/ He uses heavy aluminum foil. He is using the same kiln elements for 20 years and only does low fire and low-low fire in his kiln. If you go to NCECA he usually brings examples of his latest experiments. Two years ago, I believe it was charcoal bricquets used as an enhancer to some of the combustibles within the saggar. Look up his articles for a huge array of materials, resists and other techniques. His work was in the NCECA (Inter)national show in Louisville in 2007. Very interesting work. Marcia Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.