JRWebb Pottery Posted May 2, 2012 Report Share Posted May 2, 2012 I am looking for either a commercial glaze or a simple glaze recipe that will look sorta like white-washing. It can be semi-opaque, but I want to see the texture through it. Can be either satin or gloss finish. I work with white stoneware clay and fire to cone 6. Anyone have some ideas? Thanks! Jonni Link to comment Share on other sites More sharing options...
Mark C. Posted May 3, 2012 Report Share Posted May 3, 2012 Google White semi-opaque cone 6 glaze? the 3rd hit is a Vangilder pdf with your glazes Mark Link to comment Share on other sites More sharing options...
JRWebb Pottery Posted May 6, 2012 Author Report Share Posted May 6, 2012 Google White semi-opaque cone 6 glaze? the 3rd hit is a Vangilder pdf with your glazes Mark Thanks a bunch!! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted May 6, 2012 Report Share Posted May 6, 2012 This is one I used in reduction for decades WAXY WHITE (^6 OX) Custer feldspar 41 Silica 20 Talc 15 Gerstley Borate 15 Dolomite 7 EPK 5 103 Marcia Link to comment Share on other sites More sharing options...
JRWebb Pottery Posted May 6, 2012 Author Report Share Posted May 6, 2012 This is one I used in reduction for decades WAXY WHITE (^6 OX) Custer feldspar 41 Silica 20 Talc 15 Gerstley Borate 15 Dolomite 7 EPK 5 103 Marcia Thank you, Marcia! I'm going to mix it up and give that one a try today! Jonni Link to comment Share on other sites More sharing options...