Lynettes Posted April 14, 2012 Report Share Posted April 14, 2012 Could anyone please tell me the difference between kaolin and kaolin 6 tile. I am in Australia and we do not have kaolin 6 tile. Iam looking to trial a glaze from John Britts book, Strontium Crystal Magic. Will any type of koalin give me a result. Thank you in advance. Lynette Link to comment Share on other sites More sharing options...
Mark C. Posted April 14, 2012 Report Share Posted April 14, 2012 Could anyone please tell me the difference between kaolin and kaolin 6 tile. I am in Australia and we do not have kaolin 6 tile. Iam looking to trial a glaze from John Britts book, Strontium Crystal Magic. Will any type of koalin give me a result. Thank you in advance. Lynette I'll check my info sheet on this in am when I'm in the studio and post it.I have both materials One thing our EPK (Kaolin) is most likely from a different source than yours? Mark Link to comment Share on other sites More sharing options...
Marcia Selsor Posted April 14, 2012 Report Share Posted April 14, 2012 Go to http://wikiclay.com/wiki/kaolins Basically EPK is whiter and better in glazes and slip casting recipes. Tile 6 kaolin has titanium making an ivory color when use in clay bodies. I use Tile 6 in my raku clay. Marcia Link to comment Share on other sites More sharing options...
Mark C. Posted April 14, 2012 Report Share Posted April 14, 2012 That'a the same info I have-thanks for posting that. Mark Link to comment Share on other sites More sharing options...
neilestrick Posted April 14, 2012 Report Share Posted April 14, 2012 Tile 6 has a greater particle size distribution, and is more plastic, probably due to it's particle size distribution. It is not as white. Link to comment Share on other sites More sharing options...
Lynettes Posted April 15, 2012 Author Report Share Posted April 15, 2012 Tile 6 has a greater particle size distribution, and is more plastic, probably due to it's particle size distribution. It is not as white. Thank you for that. I thought there must have been some thing that was giving the cream colour. Now I will just do some exeriments and see what happens. Thank again. Lynette Link to comment Share on other sites More sharing options...
Recommended Posts