raddy59 Posted June 24, 2018 Report Share Posted June 24, 2018 I have a small ceramic figure with a very small footprint. I need to fix it to a wooden plinth for an exhibition submission. Glue recommendations (urgently) appreciated Link to comment Share on other sites More sharing options...
JohnnyK Posted June 24, 2018 Report Share Posted June 24, 2018 Try clear 5 minute epoxy... Link to comment Share on other sites More sharing options...
raddy59 Posted June 24, 2018 Author Report Share Posted June 24, 2018 JohnnyK - thanks for that. Any brand you recommend. Wondered I have the same issue for a larger piece, a figure that is actually vertical on one of its arms. It was ambitious I know, but a real bum of a job to mount. Think this might do the trick for that also? With that one if it fails the piece will definitely break Link to comment Share on other sites More sharing options...
Mark C. Posted June 24, 2018 Report Share Posted June 24, 2018 I like JB wield-just remember its a gray color on the fast set. for a clear glue you could could use E-6000 Link to comment Share on other sites More sharing options...
raddy59 Posted June 24, 2018 Author Report Share Posted June 24, 2018 MarK C. - E6000 - that's the smelly one, right? I'll pick up a tube and a face mask Need a clear set. Link to comment Share on other sites More sharing options...
Mark C. Posted June 24, 2018 Report Share Posted June 24, 2018 I glue outside so fumes are no issue.-E-6000 is strong stuff. Link to comment Share on other sites More sharing options...