JBaymore    1,432

Any high duty hardbrick is going to work just fine in a salt kiln for a LOT of firings.  And the more the lining gets slagging from salt buildup and erosion ....... the better the fired pots will be.  The best firing is usually the last one after you decide that this will be the last firing because the kiln is no longer safe.

The one "downside" is that a hard brick kiln or one with a hard brick lining is exopensive to fire.  On the average a hardbrick has a mass of about 8 pounds.  An insulating firebrick has a mass of about 3 pounds.  So every hardbrick that you heat up to temperature, you are heating about 5 pounds of extra material every firing.

For salt use... try to build with ah hardbrick lining and then an insulating brick outer layer (except for headers every 4th course or so).  It will lessen the firing costs over a fully hardbrick kiln.

best,

..........................john

Share this post


Link to post
Share on other sites
Rex Johnson    47

IMG_1341.PNG.79b3372ce2f96e80523d8251bf9

If this is them, still hard to tell, but hopefully not common fireplace brick often confused with refractory brick when  described as 'firebrick'.

If they are refractory bricks, I'd say yeah, and ditto the smaller kiln since it's salt and you're playing around with.

Hard refractory brick takes alot more fuel to get to temperature as compared to soft brick.

 

 

Share this post


Link to post
Share on other sites
Mark C.    1,807

The thing about determining common fireplace bricks is they are not named stamped  on sides and are more irregular in dimension and are much lower duty temp wise and should only be used in cooler chimney areas-they are also a bit more porous looking.You can see them at lumber  and building material supply stores.

Share this post


Link to post
Share on other sites
Rex Johnson    47

ditto what Mark sez...

They are cheap, usually $1.50-$2.50 new at any yard that handles cinder block and brick materials.

I have them around to use for saggars and makeshift chimneys.

IMG_4460-XL.jpg

Share this post


Link to post
Share on other sites
Marcia Selsor    1,301

yes, the stamped name is really important to trace back what type of brick you have. They look very clean as in no mortar. Saves a lot of work. I have used salvaged bricks before, and cleaning them is time consuming. Wear wrist braces when moving them bricking up hard brick doors trashed my wrists at an early age. Be protective. Firebrick s are 9" x 4.5 x 2.25" and weigh 5 lbs. each

 

Nice find

Marcia

 

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×