Any recipes for kiln furniture? I have an extruder and thought i would give it a try. I thought I saw something one time using fireclay and grog and something else. Any tips would be useful. I dont know if I can find exotic things here so I need to keep the recipe as simple as possible. I cannot find powdered fireclay here in Portugal or distributors in Spain. I must order it from the UK.

#2 Benhim

Benhim

    Advanced Member

  • Members
  • PipPipPip
  • 193 posts
  • LocationBattle Ground Washington

Posted 20 October 2011 - 05:16 PM

Any recipes for kiln furniture? I have an extruder and thought i would give it a try. I thought I saw something one time using fireclay and grog and something else. Any tips would be useful. I dont know if I can find exotic things here so I need to keep the recipe as simple as possible. I cannot find powdered fireclay here in Portugal or distributors in Spain. I must order it from the UK.




There are a number of good books to own, at the top of the list is probably 'Pioneer Pottery' by Michael Cardew which provides recipes and processes for making just about anything in the studio. Another great book to have is 'The Kiln Book' by Frederick Olsen, though I can't remember if it has a furniture recipe in it or not off hand.



I have not tested the recipe below, but intend to when I have the chance. Test and use this recipe at your own risk. It came from a forum post. It's from a reputable potter, but none the less, testing is always key.

KILN SHELF / POST BODY (^11)
Mullite(Kyanite) 60
CalcinedKaolin 20
OM#4 10
Talc10




====================


KILN WASH (Combo)

Alumina hydrate 40
EPK 30
Kyanite (35 mesh) 8
Silica 22
Fills irregularities, cleans easily.


BenCo Ceramics


#3 brigittee

brigittee

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 06 March 2013 - 05:17 AM

isn't interesting to have klin furniture.. it is like the modern design for lounge and adding more colors to lifestyle.

#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,045 posts
  • LocationGrayslake, IL

Posted 06 March 2013 - 10:08 AM

Kiln posts are cheap. Just buy some and spend your time making pots.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#5 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,430 posts
  • LocationThe Hawkeye State

Posted 06 March 2013 - 07:51 PM

Kiln posts are cheap. Just buy some and spend your time making pots.