An alternative to clay cookies is to cut soft brick into cookies.  You really need a bandsaw to do this properly, so that will probably kill this suggestion for a lot of people.  Pretty quick way to set up a box full of exact same size thickness goodness that can be used over and over.  At least until a glaze drip claims it's life.  Even then the soft brick is easier to grind than clay.