docweathers Posted February 9, 2014 Report Share Posted February 9, 2014 does anyone have a recipe for a stable clear high boron cone 6 oxidation glaze? Link to comment Share on other sites More sharing options...
Norm Stuart Posted February 9, 2014 Report Share Posted February 9, 2014 From "Mastering Cone 6 Glazes ": 100% Glossy Clear Food Safe Glaze 26% Ferro Frit 3134 26% Silica 22% Feldspar G-200 Potash 17% Kaolin - EPK 5% Talc 4% Whiting - Calcium Carbonate I have all of the glaze recipes from "Mastering Cone 6 Glazes" here http://home.roadrunner.com/~nstuart/MC6G.xls A silkier Clear "adapted from Digitalfire": 98.6% Revised - G1215U - Low Expansion Glossy Clear ^6 24.8% Kaolin 23.8% Silica 23.2% Ferro Frit 3134 15.2% Wollastonite 8.6% Feldspar F-4 Soda Minspar 200 3.0% Magnesium Carbonate does anyone have a recipe for a stable clear high boron cone 6 oxidation glaze? Link to comment Share on other sites More sharing options...
docweathers Posted February 9, 2014 Author Report Share Posted February 9, 2014 Norm you are an endless source of wisdom that spreadsheet is great too thanks Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.