dorie Posted September 26, 2010 Report Share Posted September 26, 2010 Thanks in advance! Link to comment Share on other sites More sharing options...
clay lover Posted October 1, 2010 Report Share Posted October 1, 2010 I have glossy, but not matt. Sorry. Link to comment Share on other sites More sharing options...
Brandee Ross Posted October 4, 2010 Report Share Posted October 4, 2010 Here's a nice semi-matte: http://books.google.com/books?id=PfebDtowKh0C&lpg=PA13&dq=van%20gilder%20glaze%20recipe&pg=PA131#v=snippet&q=variegated&f=false If you click on the link to page 137, you can see the recipe. Scroll up a few pages to see it in use on a pot. Link to comment Share on other sites More sharing options...