Hi, 

I am wondering if you guys have a good white clay body recommendation for throwing large forms that I will then alter.

I asked this already in another post and was told to try Soldate 60 which I will be doing I am just curious if there is a white/lighter clay body that’s good for what I’m trying to do. 
 

cheers T
 

 

Link to comment
Share on other sites

I'm using a white stoneware, IMCO "DC 3-5" ...of the several white stoneware clays I've tried, my glazes fit it; the others*, I had crazing.
How suitable it is for large forms? ...it's fine for as large as I go. It does dry well, in that it holds its shape and is less prone to cracking than many others.
 

*My glazes fit one other white stoneware I've tried, Clay Planet's "Venus White" - IMCO is closer, and we go by there several times a year...

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.