Pam S Posted September 3, 2010 Report Share Posted September 3, 2010 Does anyone have a recipe for Shino ^6 oxidation they would share? Thanks! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted September 3, 2010 Report Share Posted September 3, 2010 Here is one from MSU-Billings when I taught there. I don't know the origin. Probably a student found it somewhere. Shino ^6 Reduction Gerstley Borate 4.9 Soda Ash 2.9 Neph. Syenite 54.5 Spodumene 22.8 Ball Clay 14.9 Marcia Link to comment Share on other sites More sharing options...